Crossref journal-article
Elsevier BV
Corrosion Science (78)
Bibliography

Brass, A.-M., & Chêne, J. (2006). Hydrogen uptake in 316L stainless steel: Consequences on the tensile properties. Corrosion Science, 48(10), 3222–3242.

Authors 2
  1. A.-M. Brass (first)
  2. J. Chêne (additional)
References 40 Referenced 139
  1. {'key': '10.1016/j.corsci.2005.11.004_bib1', 'first-page': '1419', 'volume': '16-1/16-12', 'author': 'Chêne', 'year': '1980', 'journal-title': 'Bull. Cercle Et. Met.'} / Bull. Cercle Et. Met. by Chêne (1980)
  2. 10.1016/0036-9748(81)90294-5 / Scripta Metall. by Caskey (1981)
  3. {'key': '10.1016/j.corsci.2005.11.004_bib3', 'series-title': 'Current Solutions to Hydrogen Problems in Steels', 'first-page': '263', 'article-title': 'Some solutions to hydrogen embrittlement problems in Fe Ni Cr austenitic structures', 'author': 'Chêne', 'year': '1982'} / Current Solutions to Hydrogen Problems in Steels / Some solutions to hydrogen embrittlement problems in Fe Ni Cr austenitic structures by Chêne (1982)
  4. {'key': '10.1016/j.corsci.2005.11.004_bib4', 'series-title': 'Environmental Degradation of Engineering Materials in Hydrogen', 'first-page': '283', 'article-title': 'Hydrogen damage in stainless steel', 'author': 'Caskey', 'year': '1981'} / Environmental Degradation of Engineering Materials in Hydrogen / Hydrogen damage in stainless steel by Caskey (1981)
  5. 10.1016/0956-7151(90)90070-W / Acta Metall. by Rozenak (1990)
  6. 10.1016/S1359-6454(97)00349-2 / Acta Mater. by Ferreira (1998)
  7. 10.1016/0956-7151(91)90211-I / Acta Metall. by Ulmer (1991)
  8. 10.1007/BF02669643 / Metall. Mater. Trans. by Abraham (1995)
  9. 10.1007/BF02669644 / Metall. Mater. Trans. by Abraham (1995)
  10. 10.1016/S0921-5093(00)01442-8 / Mater. Sci. Eng. A by Shivanyuk (2001)
  11. {'key': '10.1016/j.corsci.2005.11.004_bib11', 'series-title': 'Hydrogen Effects on Material Behaviour and Corrosion Deformation Interactions', 'first-page': '201', 'article-title': 'Effect of hydrogen on plastic deformation of stable 18Cr–16Ni–10Mn austenitic stainless steel single crystals', 'author': 'Yagdzinskyy', 'year': '2003'} / Hydrogen Effects on Material Behaviour and Corrosion Deformation Interactions / Effect of hydrogen on plastic deformation of stable 18Cr–16Ni–10Mn austenitic stainless steel single crystals by Yagdzinskyy (2003)
  12. 10.1016/S1359-6454(02)00524-4 / Acta Mater. by Gavriljuk (2003)
  13. 10.1016/S0013-7944(00)00119-3 / Eng. Fract. Mech. by Katz (2001)
  14. G. Girardin, Thèse Ecole Nationale Supérieure des Mines de Saint-Etienne, France no. 334TD, 2004.
  15. M. Ménard, J.-M Olive, A.-M Brass, I. Aubert, Effects of hydrogen on surface slip band morphology of a type 316L stainless steel, in: Proceedings of the second NACE International Conference on Environmental-Induced cracking of metals (EICM-2), Banff, Alberta, Canada, 19–23 September 2004.
  16. 10.1016/j.corsci.2004.03.017 / Corr. Sci. by Hardie (2004)
  17. 10.1016/j.corsci.2004.07.036 / Corr. Sci. by Zackroczymski (2005)
  18. 10.1016/0022-5096(94)00056-B / J. Mech. Phys. Solids by Sofronis (2001)
  19. 10.1016/S1359-6454(02)00008-3 / Acta Mater. by Château (2002)
  20. {'key': '10.1016/j.corsci.2005.11.004_bib20', 'series-title': 'Hydrogen Effects in Metals', 'first-page': '639', 'article-title': 'Mechanisms of hydrogen related fracture of metals', 'author': 'Birnbaum', 'year': '1990'} / Hydrogen Effects in Metals / Mechanisms of hydrogen related fracture of metals by Birnbaum (1990)
  21. 10.1016/1359-6454(95)00301-0 / Acta Mater. by Magnin (1996)
  22. {'key': '10.1016/j.corsci.2005.11.004_bib22', 'series-title': 'Corrosion Sous Contrainte', 'first-page': '539', 'article-title': 'La corrosion sous contrainte des aciers inoxydables', 'author': 'Combrade', 'year': '1992'} / Corrosion Sous Contrainte / La corrosion sous contrainte des aciers inoxydables by Combrade (1992)
  23. {'key': '10.1016/j.corsci.2005.11.004_bib23', 'series-title': 'Hydrogen Effects on Materials Behaviour and Corrosion Deformation Interactions', 'first-page': '222', 'article-title': 'Interactions of hydrogen with moving dislocations in Ni base alloys. Consequences on the intergranular rupture', 'author': 'Chêne', 'year': '2003'} / Hydrogen Effects on Materials Behaviour and Corrosion Deformation Interactions / Interactions of hydrogen with moving dislocations in Ni base alloys. Consequences on the intergranular rupture by Chêne (2003)
  24. P. Tison, Influence de l’hydrogène sur le comportement des métaux, in: CEA Service de documentation, Saclay, France (Ed.), CEA-R-5240 (1), ISSN 0429-3460, 1984, pp.1–303.
  25. 10.1016/0010-938X(75)90022-0 / Corros. Sci. by Louthan (1975)
  26. 10.1007/BF02686408 / Metal Trans. by Quick (1979)
  27. 10.1016/0022-3115(88)90038-4 / J. Nucl. Mater. by Forcey (1988)
  28. J. Chêne, A.-M. Brass, in press.
  29. 10.1016/0013-4686(71)85027-2 / Electrochim. Acta by Bockris (1971)
  30. 10.1007/s11661-004-0253-y / Metall. Trans. by Brass (2004)
  31. 10.1016/0010-938X(95)00077-W / Corros. Sci. by Griffiths (1995)
  32. 10.1016/0001-6160(79)90120-2 / Acta Metall. by Miyazaki (1979)
  33. 10.1007/s11661-003-0296-5 / Metall. Mater. Trans. by Feaugas (2003)
  34. 10.1016/S0921-5093(01)01349-1 / Mater. Sci. Eng. A by Brass (2002)
  35. 10.1007/BF02817885 / Metall. Trans. A by Donovan (1976)
  36. {'key': '10.1016/j.corsci.2005.11.004_bib36', 'series-title': 'Hydrogen in Metals', 'first-page': '583', 'article-title': 'Hydrogen transport by deformation and hydrogen embrittlement in selected stainless steels', 'author': 'Chêne', 'year': '1981'} / Hydrogen in Metals / Hydrogen transport by deformation and hydrogen embrittlement in selected stainless steels by Chêne (1981)
  37. 10.1016/0022-3115(73)90121-9 / J. Nucl. Mater. by Calder (1973)
  38. {'key': '10.1016/j.corsci.2005.11.004_bib38', 'series-title': 'Hydrogen Effects on Material Behaviour', 'first-page': '19', 'article-title': 'Role of grain boundaries and cold work on hydrogen permeation in nickel', 'author': 'Brass', 'year': '1990'} / Hydrogen Effects on Material Behaviour / Role of grain boundaries and cold work on hydrogen permeation in nickel by Brass (1990)
  39. 10.1016/S0010-938X(02)00225-1 / Corros. Sci. by Li (2003)
  40. 10.1016/S1359-6454(99)00222-0 / Acta Mater. by Feaugas (1999)
Dates
Type When
Created 19 years, 8 months ago (Dec. 28, 2005, 4:59 a.m.)
Deposited 6 years, 7 months ago (Jan. 19, 2019, 12:20 a.m.)
Indexed 1 week ago (Aug. 21, 2025, 1:02 p.m.)
Issued 18 years, 10 months ago (Oct. 1, 2006)
Published 18 years, 10 months ago (Oct. 1, 2006)
Published Print 18 years, 10 months ago (Oct. 1, 2006)
Funders 0

None

@article{Brass_2006, title={Hydrogen uptake in 316L stainless steel: Consequences on the tensile properties}, volume={48}, ISSN={0010-938X}, url={http://dx.doi.org/10.1016/j.corsci.2005.11.004}, DOI={10.1016/j.corsci.2005.11.004}, number={10}, journal={Corrosion Science}, publisher={Elsevier BV}, author={Brass, A.-M. and Chêne, J.}, year={2006}, month=oct, pages={3222–3242} }