Crossref journal-article
Wiley
Surface and Interface Analysis (311)
Abstract

AbstractThe lifetime of the electrochromism of the WO3–TiO2 films prepared by vacuum evaporation is found to exceed that of WO3 films by a factor of five. X‐ray diffraction has revealed that the crystal structure of WO3–TiO2 films stays amorphous, while crystalline compounds are formed in amorphous WO3 films after colouring and bleaching. WO3–TiO2 films stay amorphous after they are annealed at 400°C, although WO3 films crystallize. SIMS and XPS analyses have revealed that half the amount of lithium injected during a colouring cycle is stored as OLi bonds in the bleached film. In WO3–TiO2 films the number of bonds such as WOH and WO in which lithium ions accumulate is reduced. We conclude that the lifetime of the electrochromism is prolonged for amorphous WO3–TiO2 films, because lithium does not accumulate and the WO3–TiO2 films stay amorphous.

Bibliography

Hashimoto, S., & Matsuoka, H. (1992). Prolonged lifetime of electrochromism of amorphous WO3–TiO2 thin films. Surface and Interface Analysis, 19(1–12), 464–468. Portico.

Authors 2
  1. Satoshi Hashimoto (first)
  2. Hideki Matsuoka (additional)
References 14 Referenced 59
  1. {'key': 'e_1_2_1_2_2', 'first-page': '177', 'volume': '36', 'author': 'Faughnan B. W.', 'year': '1975', 'journal-title': 'RCA Rev.'} / RCA Rev. by Faughnan B. W. (1975)
  2. 10.1149/1.2131429
  3. {'key': 'e_1_2_1_4_2', 'first-page': '488', 'volume': '51', 'author': 'Morita H.', 'year': '1982', 'journal-title': 'Oyo Buturi'} / Oyo Buturi by Morita H. (1982)
  4. 10.1007/BF02654669
  5. 10.1149/1.2115374
  6. 10.1149/1.2086652
  7. 10.1149/1.2085985
  8. 10.1063/1.89566
  9. {'key': 'e_1_2_1_10_2', 'first-page': '246', 'volume': '42', 'author': 'Matsuoka H.', 'year': '1991', 'journal-title': 'Hyoumen Gijutsu'} / Hyoumen Gijutsu by Matsuoka H. (1991)
  10. 10.1021/ja00784a018
  11. 10.1007/BF00882885
  12. 10.1007/BF00882886
  13. 10.1016/0167-2738(84)90006-7
  14. 10.1149/1.2127350
Dates
Type When
Created 20 years, 8 months ago (Dec. 29, 2004, 12:15 a.m.)
Deposited 2 years ago (Sept. 1, 2023, 7:01 p.m.)
Indexed 5 months, 2 weeks ago (March 19, 2025, 1:06 p.m.)
Issued 33 years, 3 months ago (June 1, 1992)
Published 33 years, 3 months ago (June 1, 1992)
Published Online 20 years, 11 months ago (Sept. 15, 2004)
Published Print 33 years, 3 months ago (June 1, 1992)
Funders 0

None

@article{Hashimoto_1992, title={Prolonged lifetime of electrochromism of amorphous WO3–TiO2 thin films}, volume={19}, ISSN={1096-9918}, url={http://dx.doi.org/10.1002/sia.740190187}, DOI={10.1002/sia.740190187}, number={1–12}, journal={Surface and Interface Analysis}, publisher={Wiley}, author={Hashimoto, Satoshi and Matsuoka, Hideki}, year={1992}, month=jun, pages={464–468} }